Type Tr-Nickel-based

3D printing Nickel-based superalloy powderIN7 18 Composition(percentage by mass) Ni Cr Nb Mo Ti Al Cu Fe 50.0-55.0 17.0-21.0 4.75-5.25 2.80-3.30 0.65-1.15 0.20-0.80 0.30 bal category Alloy grades and characteristics Alloy number: Nickel-based superalloy I

  • Data Sheets
3D printing Nickel-based superalloy powder IN718

 
Composition(percentage by mass)
Ni Cr Nb Mo Ti Al Cu Fe
50.0-55.0 17.0-21.0 4.75-5.25 2.80-3.30 0.65-1.15 0.20-0.80 ≤0.30 bal
 
category Alloy grades and characteristics
Alloy number: Nickel-based superalloy IN718 powder
Particle size: 15-45μm, 15-53μm, 53-120μm, 53-150μm
Morphology: Spherical or nearly spherical
Appearance: Grey
Package: Aluminum bag,Vacuum packing
Application: 3D printing metal powder
Other applications: powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

Packaging:Vacuum packing, 1kg/bag, or as your request.
Shipping:ASAP
  • E-mail: sales1@rboschco.com
  • Tel: 0086-0379-64280201
  • Phone: 0086-0379-65110019
  • Add: Building B, Huoju Industrial Park, Yanguang Road, Gaoxin District, Luoyang City, Henan, China.
  • Web: www.rboschco.com
  • Address:

Nanotechnology, Nano, Nanomaterials, Nanoscience, nanocatalog, nanocompany, nanoresearch, molecular manufacturing, nanotech, nanomedicine, nanometer, nanoscale, mems, nems, nanorobots, nanotubes, buckyballs, graphene, nanotechnology images, nanocomputer, self-assembly, molecular manufacturing, nanorisk, nanotoxicology, conferences, DNA, molecular machines, nanomechanics, nanoevents, future technology, nanoparticles, quantum dot, nanowire, nanofiber, companies, industries, applications, nanocompositeCopyright © 2002-2017 Luoyang Tongrun Info Technology Co., Ltd Power by DedeCms

Copyright © Luoyang Tongrun Info Technology Co., Ltd