Products

Elementary

Boride powder

Oxide powder

Sulfide powder

Hydride powder

Carbide powder

Silicide powder

Acetylacetone salt series

Myristate series

Rare Earth Chloride

Rare earth nitrate

Nitride powder

Telluride

Environmental material

3D printing materials

wafer butterfly valve

3D printing Nickel-based superalloy IN738 powder

3D printing Nickel-based superalloy IN738 powder

3D printing Nickel-based superalloy IN738 powder

Detailed

3D printing Nickel-based superalloy IN738 powder

 

Composition(percentage by mass)
 

Ni

Cr

Co

Ti

Al

Mo

Ta

Bal

14.0-16.0

8.0-9.0

2.50-4.00

2.50-1-4.00

1.00-2.00

1.00-2.00

 


 

Ta

Nb

C

Fe

 Zr

B

O

1.00-2.00

0.50-1.50

<=0.15

<=0.10

<=0.10

<=0.15

<=0.01

 


 

category

Alloy grades and characteristics

Alloy number:

Nickel-based superalloy IN738 powder

Particle size:

15-45μm, 15-53μm, 53-120μm, 53-150μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

 

 











 