3D printing Nickel-based superalloy powder nickel alloy powd

3D printing Nickel-based superalloy powder nickel alloy powd

3D printing Nickel-based superalloy powder nickel alloy powd

Detailed

Supply 3D printing Nickel-based superalloy powder nickel alloy powder  

 

category

Alloy grades and characteristics

Alloy number:

In718(GH4169),In 625(GH3625),Hastelloy X (GH3536),Waspaloy(GH738),In713C(K418),K465,K640,Rene′125(DZ125),DD6,FGH95,FGH96,FGH97

Particle size:

0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

 

7.png

8.png

 

Alloy number

Material forming process and state

Mechanical property

 

 

σb(MPa)

σ0.2(MPa)

δ(%)

IN718

Precinct laser melting/sintering heat treatment

1350-1500

1140-1280

9-20

 

Laser melt forming heat treatment state

1340-1360

1130-1170

16-28

 

Forging annealing standard reference

≥1280

≥1040

≥12

IN625

Precinct laser melting/sintering heat treatment

830-1140

550-820

30-40

 

Forging annealing standard reference

≥830

≥410

≥30

 