Supply Iron-based superalloy powder iron alloy powder 3D printing powder 

 

category

Alloy grades and characteristics

Alloy number:

Stainless steel:304,316L,410L,15-5PH,17-4PH,2Cr13;

high-strength steel:A100,300M,30CrMnSiA,40CrMnSiMoVA;

Work die steel:18Ni300,H13,M2,M35,M42,T15,2030,S390

Iron Nickel alloy powder:Invar 36

Particle size:

0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

 

Alloy number

Material forming process and state

Mechanical property

 

 

σb(MPa)

σ0.2(MPa)

δ(%)

17-4PH stainless steel powder

Precinct laser melting/sintering heat treatment

1100-1400

540-890

13-22

 

Laser melt forming heat treatment state

1080-1100

940-980

14-16

 

Forging annealing standard reference

≥930

≥725

≥10

 

.png2.jpg

Inquiry

Product:
Name:
Email:
Country:
Content:
 
Graphite powder,Nitinol powder,Nano silicon powder,Boron nitride powder,ZnS powder
  • E-mail: sales1@rboschco.com
  • Tel: 0086-18937960017
  • Phone: 0086-0379-65110019
  • Add: Building B, Huoju Industrial Park, Yanguang Road, Gaoxin District, Luoyang City, Henan, China.
  • Web: www.rboschco.com
  • Address:

Trunnano:The advanced nanomaterials supplier,Graphite powder,Nitinol powder,Nano silicon powder,Boron nitride powder,ZnS powder Power by DedeCms

Copyright © Luoyang Tongrun Info Technology Co., Ltd