Titanium-based superalloy powder for 3D printing

 

category

Alloy grades and characteristics

Alloy number:

TA0,TA1,TC4,TC4 ELI,TC11,TC17,TC18,TC21,TA7,TA12,TA15,TA17,TA19,Ti40,Ti60,TiAl(Ti36Al,Ti48Al2Cr2Nb),TiNi,TiNb,ZrTi

Particle size:

0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

 

3.png4.png

 

Inquiry

Product:
Name:
Email:
Country:
Content:
 
Graphite powder,Nitinol powder,Nano silicon powder,Boron nitride powder,ZnS powder
  • E-mail: sales1@rboschco.com
  • Tel: 0086-18937960017
  • Phone: 0086-0379-65110019
  • Add: Building B, Huoju Industrial Park, Yanguang Road, Gaoxin District, Luoyang City, Henan, China.
  • Web: www.rboschco.com
  • Address:

Trunnano:The advanced nanomaterials supplier,Graphite powder,Nitinol powder,Nano silicon powder,Boron nitride powder,ZnS powder Power by DedeCms

Copyright © Luoyang Tongrun Info Technology Co., Ltd